Tipco Tipcolene® UV 1006 - Combination of UV Stabilizer & UV Absorber Masterbatch with 15% UV & Anti-Oxidants in LDPE

Category Polymer
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® UV 1006 - Combination of UV Stabilizer & UV Absorber Masterbatch with 15% UV & Anti-Oxidants in LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
1.10 g/cc
0.0397 lb/in³
ASTM D792
Apparent Bulk Density 0.500 g/cc
0.0181 lb/in³
TRM-37
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238