Material Notes:
Made by suspension polymerization. APPLICATIONS Extrusion : - plasticized, semi-rigid and rigid profiles - plasticized and rigid pipes - rigid "pressure" pipes Injection molding : plasticized and semi-rigid products Calendering : plasticized and semi-rigid opaque films and sheetsInformation provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density 0.500 g/cc
0.0181 lb/in³
ISO 60
Particle Size 63 µm
63 µm
>93% greater than value; ISO 1624
250 µm
250 µm
<2% greater than value; ISO 1624
Viscosity Test 102 cm³/g
102 cm³/g
Reduced viscosity, K value = 64; ISO 1628-2