Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.78 g/cc | 0.0643 lb/in³ | |
Poco Graphite AXF-5F Biomedical Grade Graphite POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin.. |
|||
Apparent Bulk Density | 1.78 g/cc | 0.0643 lb/in³ | |
Poco Graphite ZXF-5Q Industrial Grade Graphite SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Apparent Bulk Density | 1.78 g/cc | 0.0643 lb/in³ | |
Ohio Carbon Blank OCB AR-12 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Apparent Bulk Density | 1.78 g/cc | 0.0643 lb/in³ | |
Poco Graphite AXF-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Apparent Bulk Density | 1.78 g/cc | 0.0643 lb/in³ | |
Ohio Carbon Blank OCB TTK-4 EDM Grade Graphite Available in a range of sizes and shapes. |