Material Notes:
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal graphite to each application. Post synthesis modifications enhance the original material to allow even greater flexibility for highly specialized conditions.
Physical Properties Metric English Comments
Apparent Bulk Density 1.78 g/cc
0.0643 lb/in³
Open Porosity 80 %
80 %
Porosity 20 %
20 %
Particle Size 5.0 µm
5.0 µm
Pore Size 0.800 microns
0.0315 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Tensile Strength, Yield 62.0 MPa
8990 psi
Elongation at Yield 0.95 %
0.95 %
Modulus of Elasticity 11.0 GPa
1600 ksi
Flexural Strength 86.0 MPa
12500 psi
Compressive Strength 138 MPa
20000 psi
Thermal Properties Metric English Comments
CTE, linear 7.90 µm/m-°C
4.39 µin/in-°F
Thermal Conductivity 95.0 W/m-K
659 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00147 ohm-cm
0.00147 ohm-cm