Poco Graphite AXF-5F Biomedical Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite AXF-5F Biomedical Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineering support, precision machining, and material testing. Diverse applications include precision parts, graphite filters for blood dialysis machines, graphite electrodes and heating elements.The compatibility of carbon and graphite with human tissues and bodily fluids have allowed POCO materials to be used in a variety of implants. Applications include artificial heart valves, dental mounts, cancer treatment devices and blood analysis devices.
Physical Properties Metric English Comments
Apparent Bulk Density 1.78 g/cc
0.0643 lb/in³
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Flexural Strength 90.0 MPa
13100 psi
Compressive Strength 145 MPa
21000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 95.0 W/m-K
659 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00147 ohm-cm
0.00147 ohm-cm