Physical Properties Metric English Comments
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
Geon® STP 1169; Internal Method
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan..
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
Geon® STP 1169; Internal Method
PolyOne Geon™ Specialty Suspension Impel S100 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Impel S100 is a homopolymer specialty suspension resin intended for use in highly plasticized extrusion and injection molding formulations. It gives superior plasticizer absorption properties..
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE)
Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with..
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE)
Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low ..
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite  (discontinued **)
Data provided by the manufacturer.35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p..