Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with high filler content. This material exhibits high bulk density, tensile strength and elongation at break. Black compounds based on Algoflon® F5/S show optimum isotropic behavior and therefore excellent longitudinal mechanical properties.Features: Good Chemical ResistanceUses: Additive; BlendingInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
ASTM D792
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
ASTM D4894
Water Absorption 0.00 %
0.00 %
ASTM D570
Particle Size 15 µm
15 µm
Internal Method
Linear Mold Shrinkage 0.031 cm/cm
0.031 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Flammability, UL94 V-0
V-0
VE-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 60.0 - 2.00e+9 Hz
2.1

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150
Dielectric Strength 70.0 kV/mm
1780 kV/in
Estimated from similar grades. ASTM D149
Dissipation Factor >= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
>= 0.00030

@Frequency 60.0 - 2.00e+9 Hz
ASTM D150
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1550
Availability Asia Pacific; Europe
Color White
Form Powder
Users viewing this material also viewed the following: