Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® 35CAR PTFE; Petroleum Coke and Graphite  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.35 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.09 g/cc
0.0755 lb/in³
ASTM D792
Apparent Bulk Density 0.410 g/cc
0.0148 lb/in³
ASTM D4894
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature 23.0 - 250 °C
72.2 µin/in-°F

@Temperature 73.4 - 482 °F
ASTM D696
Thermal Conductivity 0.620 W/m-K
4.30 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Electrical Properties Metric English Comments
Electrical Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Users viewing this material also viewed the following: