Material Notes:
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistance property.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
Dried at 110°C
Grain Size <= 6000 µm
<= 6000 µm
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00441 GPa

@Temperature 1100 °C
0.640 ksi

@Temperature 2010 °F
0.00931 GPa

@Temperature 110 °C
1.35 ksi

@Temperature 230 °F
0.0108 GPa

@Temperature 1500 °C
1.57 ksi

@Temperature 2730 °F
Compressive Strength 0.0981 MPa

@Temperature 1000 °C
14.2 psi

@Temperature 1830 °F
Cold Crushing
0.196 MPa

@Temperature 110 °C
28.4 psi

@Temperature 230 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 0.105 W/m-K
0.729 BTU-in/hr-ft²-°F
1.28 W/m-K
8.88 BTU-in/hr-ft²-°F
1.37 W/m-K
9.51 BTU-in/hr-ft²-°F
1.45 W/m-K
10.1 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Fe2O3 11 %
11 %
Descriptive Properties Value Comments
Permanent Linear Change <-0.06%
800°C
<-0.08%
1500°C
<-0.12%
1100°C
-0.8 - 0.8%
1000°C
Refractoriness <1800°C