Physical Properties Metric English Comments
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Viscosity 70 - 100 cP
70 - 100 cP
Huntsman AroCy L-10 Cyanate Ester
Comments/Applications: Max color is 8. Lowest viscosity liquid cyanate ester. Used in filament winding, RTM, pultrusion. Can also be used as a viscosity modifier in other cyanate ester systems.Da..
Viscosity 70 cP
70 cP
KKPC KOSYN KSL 203 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro..
Viscosity 70 cP
70 cP
KKPC KOSYN KSL 201 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro..
Viscosity 70 cP
70 cP
B-type viscometer (60rpm)
Mitsui UNISTOLEâ„¢ R-120K Polyolefinic Primer/ Adhesive
UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi..
Viscosity 70 - 130 cP
70 - 130 cP
15% solids in MEK
Taiwan Sheen Soon Sheenthane® AS-120 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use..
Viscosity 70 - 130 cP
70 - 130 cP
15% solids in MEK
Taiwan Sheen Soon Sheenthane® AS-120L TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use..
Viscosity 70 cP

@Temperature 25.0 °C
70 cP

@Temperature 77.0 °F
Shin-Etsu Silicones Primer 33
Primer No. 33 is a reddish brown colored primer designed for bonding HCR/silicone rubber to plastics and metals such as aluminum, stainless steel, and iron. Use: Metal substratum surface must be cl..
Viscosity 70 - 120 cP
70 - 120 cP
Master Bond UV15LV One Component, UV Curable Epoxy Based System
Product Description: Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It has low viscosity and it is widely used in a variety of ..
Viscosity 70 - 80 cP

@Temperature 20.0 °C
70 - 80 cP

@Temperature 68.0 °F
4% solids aqueous solution, Hoeppler falling ball method
DuPont Elvanol® 70-75 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..
Viscosity 70 - 120 cP
70 - 120 cP
HY2954 cycloaliphatic amine hardener; DIN 53015
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.
Viscosity 70 cP
70 cP
dynamic
Dow Corning TM-1950 EMULSION
Dow Corning® TM-1950 Emulsion and Dow Corning® TM-1951 Emulsion are water-based silicone products with excellent dilution stability, which provide release of tissue paper from felt, fabric and wir..
Viscosity 70 cP
70 cP
Dow PAPI™ 95 Polymeric MDI
PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan..
Viscosity 70 - 130 cP
70 - 130 cP
3M Scotch-Weld™ CA8 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3..
Viscosity 70 cP

@Temperature 70.0 °C
70 cP

@Temperature 158 °F
at 100/28 (50-6/50-17) pbw
Abatron AboCast 50-6/AboCure 50-17 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months.
Viscosity 70 - 120 cP
70 - 120 cP
3M Pronto™ CA-8 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting adhesive with exce..
Viscosity 70 cP
70 cP
BASF Lupranate® M10 Isocyanate
Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level ..