Material Notes:
Kraton D1101 K is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:Kraton D1101 KT - supplied as a dusted porous pelletKraton D1101 KU - supplied as an undusted porous pelletKraton D1101 KIM - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America and South AmericaUses: Kraton D1101 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.Note 1: The final dusting level is a combination of the talc from the original D1101 KT plus calcium carbonate added during the milling process.Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D402
Volatiles <= 0.70 %
<= 0.70 %
KM 04
Viscosity 3900 cP
3900 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.15 - 0.35 %
0.15 - 0.35 %
KT, Talc; BAM 908
4.0 - 6.0 %
4.0 - 6.0 %
KIM, See note 1; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 69

@Time 10.0 sec
69

@Time 0.00278 hour
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 31.7 MPa
4600 psi
measured on films cast from a solution in toluene; ASTM D412
Elongation at Break 880 %
880 %
Measured on films cast from a solution in toluene; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 16 %
16 %
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.15-0.4%, KM 08
Polystyrene
39-33%, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 31/69