Material Notes:
Carbon Graphite Ink is used for screen printing working electrodes. This is a carbon graphite ink, which has been optimized to give superior electrochemical performance with good reversibility when using cyclic voltammetry. For optimum print properties and fine lines we would recommend the use of Carbon/Graphite C2000802D2.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Viscosity 3900 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
3900 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Thickness 13.0 microns
0.512 mil
printed through a 230 mesh SS screen with 13 micron emulsion back off
Storage Temperature 20.0 °C
68.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 45 ohm
45 ohm
cured film; 13 microns thick
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 820
230 mesh stainless steel screen with 13 micron emultion back off
Printing Mesh counts/inch 150 to 250
stainless steel or polyester screens