Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 35 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 35 - 60 cP
35 - 60 cP
ND Industries 306 Surface Insensitive Instant Superglue
Low viscosity for difficult to bond rubber compounds
Viscosity 35 - 60 cP
35 - 60 cP
3
ND Industries SuperGlue Ethyl 395
General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen..
Viscosity 35 - 45 cP
35 - 45 cP
Liquid State
Palm Labs Adhesives Turbo Fuse Series 120 (40 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 35 - 45 cP
35 - 45 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 120 LOW ODOR/LOW BLOOM (40 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p..
Viscosity 35 - 45 cP
35 - 45 cP
Liquid State
Palm Labs Adhesives Turbo Fuse Series 120SI Surface Insensitive (40 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th..
Viscosity 35 cP
35 cP
5% Toluene Solution; ASTM D445
LG Chemical LG-428N Styrene-Butadiene-Styrene
Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem..
Viscosity 35 - 100 cP
35 - 100 cP
ASTM D445
IRPC Polimaxx Polene PE220NSC Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Viscosity 35 cP

@Temperature 200 °C
35 cP

@Temperature 392 °F
Melt
Unitika elitel UE3230 Polyester, Flake
Adhesive agent, Resin modifierUNITIKA elitel resins are thermoplastic saturated copolymeric polyester resins. Elitel resins are expanding their applications from products such as adhesives, paints,..
Viscosity 35 - 60 cP

@Temperature 25.0 °C
35 - 60 cP

@Temperature 77.0 °F
Mixed
Trelleborg Emerson & Cuming Eccobond® 11 Heat Cure Catalyst
Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to ..
Viscosity 35 cP
35 cP
(mixed)
Loctite® Shadowcure™ 394 Acrylic/urethane UV Coating
Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti..
Viscosity 35 cP

@Temperature 25.0 °C
35 cP

@Temperature 77.0 °F
Value represents initial mixed viscosity of components.
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Viscosity 35 cP
35 cP
BASF Lupranate® 230 Isocyanate
Description: Lupranate® 230 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio..
Viscosity 35 cP
35 cP
BASF Lupranate® 245 Isocyanate
Description: Lupranate® 245 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (pure MDI)In..
Viscosity 35 cP
35 cP
B Component; ASTM D1824
Aptek 2100-A7C/B Low modulus urethane staking compound
APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Althoug..
Viscosity 35 cP
35 cP
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder
A colloidal silica aqueous solution which produces high adhesive strength. Ideal for blending with all types of granular and fibrous ceramics. Excellent resistance to temperature, moisture and mecha..