Unitika elitel UE3230 Polyester, Flake

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Unitika
Trade Name elitel
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika elitel UE3230 Polyester, Flake.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders, and modifying agents to the products in new-generation high-tech fields.Characteristics:l products have superior adhesiveness and coatability. They exhibit excellent adhesiveness and coatability to films and molded products of plastic materials such as polyester, polyvinylchloride, polycarbonate, and cellulose acetate; steel materials such as steel plates; metal materials such as copper, and aluminum; woven or nonwoven fabrics from polyester and other fibers; papers, woods, and others.l products may be hardened by combined use of a hardening agent.Blending of an l resin with another l resin or a different resin provides alloys with more diversified resin properties. Additionally, l products are effective as a modifying resin for providing other resins with flexibility, coatability, toughness, and others. l resins form films excellent in flexibility, electrical properties, weather resistance, as well in appearance and transparency: l resins retain consistent quality with smaller change in quality over time They are also excellent hygienically.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
JIS K-6911
Moisture Absorption at Equilibrium 0.50 %
0.50 %
60%RH
Viscosity 35 cP

@Temperature 200 °C
35 cP

@Temperature 392 °F
Melt
Viscosity Measurement 0.71
0.71
Limiting Viscosity
Molecular Weight 20000 g/mol
20000 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
Tensile Strength at Break 0.300 MPa
43.5 psi
ASTM D638
Elongation at Break 1000 %
1000 %
ASTM D638
Thermal Properties Metric English Comments
Softening Point 115 °C
239 °F
JIS K-2531
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Electrical Properties Metric English Comments
Dielectric Constant 6.0
6.0
ASTM D150
Dissipation Factor 0.065
0.065
ASTM D150
Chemical Properties Metric English Comments
Acid Value 1.0
1.0
[mgKOH/g}
Descriptive Properties Value Comments
Appearance Yellowish green
Hydroxyl Value 5 mgKOH/g