Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pigment dispersion aid in polypropylene fiber applications. As a paraffin wax modifier it improves blocking, scuff, and abrasion resistance. Key Attributes: Improves blocking, scuff, and abrasion resistance in paraffin wax blendsLow molecular weightPolypropylene (PP) homopolymerUseful in color concentrates, toner compounds, and as a pigment dispersion aid Application/Uses:Building and ConstructionHot Melt AdhesivesPackagingSolventborne AdhesivesWax Modification
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D5
Viscosity 250 - 950 cP

@Temperature 190 °C
250 - 950 cP

@Temperature 374 °F
542-111
Brookfield Viscosity 700 cP

@Temperature 190 °C
700 cP

@Temperature 374 °F
ASTM D3226
Molecular Weight 12000 g/mol
12000 g/mol
Thermal Properties Metric English Comments
Flash Point >= 277 °C
>= 531 °F
Ring & Ball Softening Point 163 °C
325 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
542-130
Descriptive Properties Value Comments
Penetration Hardness <1 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm