Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 700 - 900 cP @Temperature 23.0 °C |
700 - 900 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-033 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-031 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-058 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-064 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PPA-019 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7120 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 cP | 700 cP | ASTM D2293 |
Fibre Glast Epolite 2427 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Viscosity | 700 - 527068 cP @Temperature 230 - 280 °C |
700 - 527068 cP @Temperature 446 - 536 °F |
Average value: 221000 cP Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Viscosity | 700 cP | 700 cP | KM 06 |
Kraton® D1155 E (SBS) Liner Block Copolymer Description: Kraton D1155 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Europe in the physical form identified: Kraton D1155.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1163 B (SIS) Linear Block Copolymer Description: Kraton D1163 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Huntsman PY 258 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 185 to 196. Max color is 3.Comments/Applications: Provides excellent heat and chemical resistance especially in post bake or heat cured coatings. Chemically modified.. |
|||
Viscosity | 700 cP | 700 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi.. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours .. |
|||
Viscosity | 700 cP @Temperature 23.0 °C |
700 cP @Temperature 73.4 °F |
|
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy Master Bond Polymer System EP29LPSP is a two component, high performance, modified low temperature heat cured epoxy system specially formulated for cryogenic applications. EP29LPSP is serviceable at.. |
|||
Viscosity | 700 cP | 700 cP | |
Loctite® Tak Pak® 444 Instant Adhesive Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackersLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of.. |
|||
Viscosity | 700 - 1000 cP | 700 - 1000 cP | NOV QC 020 |
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 700 cP | 700 cP | |
Dow Corning SYL-OFF® 7138 HIGH SPEED CROSSLINKER Syl-Off® 7138 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr.. |
|||
Viscosity | 700 - 1200 cP @Temperature 23.0 °C |
700 - 1200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Viscosity | 700 cP | 700 cP | dynamic |
Dow Corning 593 FLUID Blend of polydimethylsiloxane and high molecular weight silicone resin.Information provided by Dow Corning |
|||
Viscosity | 700 cP | 700 cP | |
BASF Lupranate® M70L Isocyanate Description: Lupranate® M70L Isocyanate is a solvent-free, medium-viscosity polymethylene polyphenypolyisocyanate. Lupranate M70L Isocyanate, having a higher viscosity than Lupranate M20S, is parti.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem WSR615 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
Uncured |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |
|||
Viscosity | 700 cP @Temperature 200 °C |
700 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3500 Polyester, Flake High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc.. |