Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.0 cP | 3.0 cP | |
ND Industries 611 Heptane-Acetone Anaerobic Primer General purpose anaerobic primer. On part life 30 days. Non-ozone depleting but flammable solvent |
|||
Viscosity | 3.0 cP | 3.0 cP | |
ND Industries 612 Heptane-Acetone Anaerobic Primer Fast acting anaerobic primer. On part life 7 days. Non-ozone depleting but flammable solvent |
|||
Viscosity | 3.0 cP | 3.0 cP | ASTM D2196 |
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Viscosity | 3.0 - 10 cP @Temperature 25.0 °C |
3.0 - 10 cP @Temperature 77.0 °F |
Uncured |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Viscosity | 3.0 cP | 3.0 cP | ASTM D2196 |
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Viscosity | 3.0 cP | 3.0 cP | DIN 54 453; D=4000/s |
3M Dyneon™ TF 5033 PTFE Dispersion
(discontinued **) 35% Solids; 4% Ionic emulsifier (solids basis). Used for metal composite bearings.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application.. |
|||
Viscosity | 3.0 - 15 cP | 3.0 - 15 cP | |
Solvay AMGARD® TOF Phosphorus Derivative Chemical Name: TRIOCTYL PHOSPHATE (TOF)CAS: 78-42-2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: AMGARD TOF is a halogen free phosphate plasticizer with a very goo.. |
|||
Viscosity | 3.0 - 4.0 cP @Temperature 20.0 °C |
3.0 - 4.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-03 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 3.0 - 4.0 cP @Temperature 20.0 °C |
3.0 - 4.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-03 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 417 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 7090 No solvent Base Surface Primer Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 7109 Perfluorocarbon Base Surface Primer Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 736 Trichloroethylene isopropyl alcohol Base Surface Primer Loctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the cure speed and ga.. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
Loctite® 793 Propylene based glycol ether/water Base Surface Primer Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Viscosity | 3.0 - 7.0 cP | 3.0 - 7.0 cP | |
Daikin NEOFLON ND-4 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Viscosity | 3.0 - 7.5 cP | 3.0 - 7.5 cP | |
Daikin NEOFLON ND-4GY FEP Dispersion, Gray NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Viscosity | 3.0 cP @Temperature 25.0 °C |
3.0 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT T 100 TDI 100 isocyanate Description of product:Appearance: At room temperature water clear liquid. Composition: The concentration 2,4-toluene-di-isocyanate is min. 97 w/w %.The product contains beside this mainly 2,6-tolue.. |
|||
Viscosity | >= 3.0 cP | >= 3.0 cP | |
3M Scotch-Weld™ AC77 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC77 is designed for difficult-to-bond, low surface energy plastics such as polypropylene, polyethylene, and PTFE. This primer needs to be applied to each .. |
|||
Viscosity | 3.0 - 8.0 cP | 3.0 - 8.0 cP | U-Tube IC-C45 |
3M Scotch-Weld™ MG05 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Viscosity | 3.0 cP | 3.0 cP | |
3M Scotch-Weld™ MG77 AC Medical Grade Instant Adhesive Primer 3M™ Scotch-Weld™ Medical Grade Instant Adhesive Primers are liquid chemical products used in conjunction with 3M™ Scotch-Weld™ Medical Grade Instant Adhesives. MG77 AC is a cyanoacrylate primer .. |
|||
Viscosity | 3.0 cP @Temperature 25.0 °C |
3.0 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT T 65 TDI 65/35 Isocyanate Description of product:Appearance: At room temperature water clear liquid.Composition: A mixture of toluene diisocyanate isomers (2,4-toluene diisocyanate [A] and 2,6-toluene diisocyanate [B]. Nomin.. |
|||
Viscosity | 3.0 cP @Temperature 25.0 °C |
3.0 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT T 80 TDI 80/20 Isocyanate Description of product:Appearance: At room temperature water clear liquid. Composition: A mixture of toluene-di-isocyanate isomers (2,4-toluene-di-isocyanate [A] and 2,6-toluene-di-isocyanate [B].No.. |