Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.2 cP | 1.2 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® 28 PVC PVC Homopolymer Dispersion Resin F-28 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities as well as low residual surfactant content. This product was de.. |
|||
Viscosity | 1.2 cP | 1.2 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® 38 PVC PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properti.. |
|||
Viscosity | 1.2 cP | 1.2 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® KVH PVC PVC Homopolymer Dispersion Resin F-KVH is a structured high molecular weight PVC homopolymer dispersion resin which imparts pseudoplastic flow in which it is used. Plastisol prepared utilizing F-KVH.. |
|||
Viscosity | 1.2 cP | 1.2 cP | |
3M Novec™ 4300 Electronic Surfactant 3M™ Novec™ 4300 Electronic Surfactant is an anionic fluorochemical surfactant available as a 20 wt% solution in glacial acetic acid with low metal content, typically containing < 30 ppm of each sp.. |