Formosa Plastics Formolon® KVH PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® KVH PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Homopolymer Dispersion Resin F-KVH is a structured high molecular weight PVC homopolymer dispersion resin which imparts pseudoplastic flow in which it is used. Plastisol prepared utilizing F-KVH are particularly suited for dip, slush and rotational molding where mold release and pseudoplasticity are desired as well as fabric coating application where minimum strike through is essential.Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Volatiles 0.30 %
0.30 %
ASTM D3030
Viscosity 1.2 cP
1.2 cP
Inherent; ASTM D1243
8000 cP
8000 cP
Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.65 cP
2.65 cP
QC-10-104
Brookfield Viscosity 60000 cP
60000 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
500000 cP
500000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Descriptive Properties Value Comments
Composition 0.015
Methanol Extract, ASTM D2222
Gelation Temperature 175°F
SPI-VD-T18
K-Value 75
Fikentscher's Constant