3M Novec™ 4300 Electronic Surfactant

Category Fluid
Manufacturer 3M
Trade Name Novec™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Novec™ 4300 Electronic Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Novec™ 4300 Electronic Surfactant is an anionic fluorochemical surfactant available as a 20 wt% solution in glacial acetic acid with low metal content, typically containing < 30 ppm of each specified metal. Novec 4300 surfactant provides low surface tensions in low pH solutions, such as Phosphoric/Acetic/Nitric Acid mixtures for metal etching. It also provides low surface tension in a variety of other aqueous solutions. Novec 4300 surfactant offers : Improved wetting Good solubility Low effective concentration Stability in bath FilterabilityOn the basis of toxicity testing conducted on Novec 4300 surfactant and life cycle assessment of its intended applications, 3M characterizes Novec 4300 surfactant as sustainable technology. Additional EHSR data on this product is available from 3M.Typical Applications: For use in metal etch solutions including Phosphoric/Acetic/Nitric ("PAN Etch") blends, and in other aqueous microelectronic process chemicals including low pH solutionsInformation provided by 3M
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Viscosity 1.2 cP
1.2 cP
Descriptive Properties Value Comments
Color Clear, colorless liquid
Type Anionic