Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 38 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properties which permits utilization of this product in a variety of applications including dip coating, slush and roto-casting, in addition to both solid and expanded fabric coating constructions.Note 1. 500 gm resin and 300 gm DOP, Hobart mixer mixed 5 min. @ No. 1 speed and 10 min. @ No. 2 speed, undeaerated.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Volatiles 0.30 %
0.30 %
ASTM D3030
Viscosity 1.2 cP
1.2 cP
Inherent; ASTM D1243
12000 cP
12000 cP
Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2
Relative Viscosity 2.65 cP
2.65 cP
QC-10-104
Brookfield Viscosity 5500 cP
5500 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
10000 cP
10000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Descriptive Properties Value Comments
Composition 0.025
Methanol Extract, ASTM D2222
Gelation Temperature 168°F
SPI-VD-T18
K-Value 75
Fikentscher's Constant