Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0040 - 0.0050 cm/cm @Thickness 6.35 mm |
0.0040 - 0.0050 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 - 0.0050 cm/cm @Thickness 3.17 mm |
0.0040 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0050 cm/cm @Thickness 3.17 mm |
0.0040 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/15/UV/HS Polypropylene Homopolymer, 15% Glass Reinforced, Heat Stabilized, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.17 mm |
0.0030 - 0.0050 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 1.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0050 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm @Thickness 1.00 mm |
0.0030 - 0.0050 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
aged 48 hrs at 121°C; ISO 294 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |