Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0145 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
Plastcom SLOVAMID 6 GF 30 HI PA6, 30% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength a..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Linear Mold Shrinkage, Transverse 0.0145 - 0.016 cm/cm

@Thickness 3.17 mm
0.0145 - 0.016 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66UT105 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Linear Mold Shrinkage, Transverse 0.0145 - 0.016 cm/cm

@Thickness 3.17 mm
0.0145 - 0.016 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66UT108 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Linear Mold Shrinkage, Transverse 0.0145 - 0.016 cm/cm

@Thickness 3.17 mm
0.0145 - 0.016 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66UT119 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
Annealed; ISO 294-4
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
STN 64 0808
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant
Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0185 cm/cm
0.0145 - 0.0185 in/in
LATI Latigray 52/11-01 CX/45 PP Homopolymer
Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
annealed; ISO 294-4
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Linear Mold Shrinkage, Transverse 0.0145 - 0.0175 cm/cm
0.0145 - 0.0175 in/in
LATI Latiohm 52/11-10 PD02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
STN 64 0808
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application ..
Linear Mold Shrinkage, Transverse 0.0145 cm/cm
0.0145 in/in
Plastcom SLOVAMID 6 NG GF 30 LS PA6, 30% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..