Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead HSD12 Normal Grade Heat Sealable Film (thickness: 18 µm) HSD12 is a printing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona trea.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM-D1204 |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.0205 cm/cm | 0.018 - 0.0205 in/in | |
LATI Latilub 75/4-20T PBT, PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | 0.125 in; ASTM D955 |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | DIS 294-4 |
Wellman Wellamid® 22LHI4 XE-GY1 Nylon 66, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | 60x60x4; ISO 294-4 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, Conditioned Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190 Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. Available in Natural and Black. Natural: Designated RH190N-3; Black: Designated RH190B.Data provid.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.0205 cm/cm | 0.018 - 0.0205 in/in | |
LATI Later 4E61 PBT Polybutylene Terephthalate (PBT). Toughened. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t.. |