Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.021 - 0.022 cm/cm
0.021 - 0.022 in/in
ASTM D955
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.013 - 0.022 cm/cm

@Thickness 3.18 mm
0.013 - 0.022 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Linear Mold Shrinkage, Transverse 0.021 - 0.022 cm/cm
0.021 - 0.022 in/in
ASTM D955
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.0195 - 0.022 cm/cm
0.0195 - 0.022 in/in
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Linear Mold Shrinkage, Transverse 0.020 - 0.022 cm/cm

@Thickness 3.20 mm
0.020 - 0.022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 305 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850.
Linear Mold Shrinkage, Transverse 0.020 - 0.022 cm/cm

@Thickness 3.20 mm
0.020 - 0.022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 308 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.020 - 0.022 cm/cm

@Thickness 3.20 mm
0.020 - 0.022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 309 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only.
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm

@Thickness 3.20 mm
0.018 - 0.022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® HX3091HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only.
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO DIS 294-4
Wellman Wellamid® 22LHI3 XE-NBK1 Impact Modified Engineering Nylon 66
Description: Impact Modified Engineering Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
DIS 294-4
Wellman Wellamid® 22LHI4 XE-GY1 Nylon 66, Impact Modified
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
DIS 294-4
Wellman Wellamid® NY1875-BK1 Nylon 66, Unfilled
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Solvay TECHNYL® 2210HS PA66, DRY
Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe..
Linear Mold Shrinkage, Transverse 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO DIS 294-4
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.