Polymer Property : Filament Diameter = 14 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Filament Diameter 14 µm
14 µm
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
Filament Diameter 14 µm
14 µm
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber
Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus..
Filament Diameter 14 µm
14 µm
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
Filament Diameter 14 - 26 µm
14 - 26 µm
AGY VeTron® Glass Fiber
Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp.