Material Notes:
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties for ceramic fibers, and retains its properties at high temperatures. Nicalon™ is highly resistant to oxidation and chemical attack.Product Forms:Continuous Fiber: Supplied as multi-filament tow, spooled on 3 inch ID bobbins to 500 meters in length (100 grams in weight). Also available in random lengths at a reduced price.Woven Cloth: Available in three weave styles as shown in Table 2. Woven cloth is typically supplied as 1-meter-wide continuous rolls of specific lengths. Other weave or braid styles can be made available.Chopped Fiber: Available of 1-mm length chopped multi-filament tow. Longer lengths also available. Packaged as 3 kg containers.Felt / Mat: Random lengths of Nicalon™ ceramic fiber in a PVA binder. Customizable areal weights, shapes and sizes.Uses: Nicalon™ ceramic fiber can be used as a reinforcement for plastic, ceramic, and metal matrix composites to produce high performance composite materials. Surface treatments are normally recommended to facilitate processing and maximize composite properties Nicalon™ can also be used to form fibrous products such as high temperature insulation, filters, etc. Its resistance to chemical attack allows it to be used in harsh environments. The standard grade of the Nicalon™ product line; offers the optimum mechanical properties and high temperature performance for most applications.Information from COI Ceramics, Inc.
Physical Properties Metric English Comments
Density 2.55 g/cc
0.0921 lb/in³
Filament Diameter 14 µm
14 µm
Fiber Count 2000 dtex
1800 denier
Mechanical Properties Metric English Comments
Tensile Strength 3000 MPa
435000 psi
Tensile Modulus 210 GPa
30500 ksi
Thermal Properties Metric English Comments
CTE, linear 3.20 µm/m-°C

@Temperature 25.0 - 500 °C
1.78 µin/in-°F

@Temperature 77.0 - 932 °F
3.90 µm/m-°C

@Temperature 900 °C
2.17 µin/in-°F

@Temperature 1650 °F
Specific Heat Capacity 0.710 J/g-°C

@Temperature 25.0 °C
0.170 BTU/lb-°F

@Temperature 77.0 °F
1.17 J/g-°C

@Temperature 500 °C
0.280 BTU/lb-°F

@Temperature 932 °F
Thermal Conductivity 2.20 W/m-K

@Temperature 500 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 932 °F
2.97 W/m-K

@Temperature 25.0 °C
20.6 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Component Elements Properties Metric English Comments
Carbon, C 32 %
32 %
Oxygen, O 12 %
12 %
Silicon, Si 57 %
57 %
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
Dielectric Constant 9.2
9.2
Descriptive Properties Value Comments