COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber

Category Ceramic , Carbide
Manufacturer COI Ceramics
Trade Name Nicalon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus properties. HI-Nicalon™ is highly resistant to oxidation and chemical attack and is available in a variety of product forms, depending on the intended use.The fiber is coated with polyvinyl alcohol (PVA) sizing for improved handling.Special Properties: CMC’s reinforced with HI-Nicalon™ ceramic fiber offers distinct advantages over other materials. Oxide fiber and superalloys generally lose mechanical properties above 800C. SiCO fiber generally loses properties above 1000C. 100 micron diameter monofilament SiC fiber is generally not weavable. HI-Nicalon™ ceramic fiber overcomes these drawbacks. Product Forms:Continuous Fiber: Supplied as multi-filament tow, spooled on 3 inch ID bobbins to 500 meters in length (100 grams in weight). Also available in random lengths at a reduced price.Woven Cloth: Available as Plain Weave, 5HS Weave or 8HS Weave, HI-Nicalon™ cloth is typically supplied as 1 meter-wide continuous rolls of specific lengths. Other widths weave or braid styles can be made available.Chopped Fiber: Available as 1-mm length chopped multi-filament tow. Longer lengths also available.Uses: HI-Nicalon™ ceramic fiber is primarily designed to be used as reinforcements for high temperature ceramic composites. It can also be used as a reinforcement for plastic, and metal matrix composites. Surface treatments are normally recommended to facilitate processing and maximize composite properties. The fiber can also be used to form fibrous products such as high temperature insulation, filters, etc. Its resistance to chemical attack allows it to be used in harsh environments.Information from COI Ceramics, Inc.
Physical Properties Metric English Comments
Density 2.74 g/cc
0.0990 lb/in³
Filament Diameter 14 µm
14 µm
Fiber Count 2000 dtex
1800 denier
Mechanical Properties Metric English Comments
Tensile Strength 2800 MPa
406000 psi
Tensile Modulus 270 GPa
39200 ksi
Thermal Properties Metric English Comments
CTE, linear 3.50 µm/m-°C

@Temperature 25.0 - 500 °C
1.94 µin/in-°F

@Temperature 77.0 - 932 °F
Specific Heat Capacity 0.670 J/g-°C

@Temperature 25.0 °C
0.160 BTU/lb-°F

@Temperature 77.0 °F
1.17 J/g-°C

@Temperature 500 °C
0.280 BTU/lb-°F

@Temperature 932 °F
Thermal Conductivity 7.77 W/m-K

@Temperature 25.0 °C
53.9 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
10.1 W/m-K

@Temperature 500 °C
70.1 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Carbon, C 37 %
37 %
Oxygen, O 0.50 %
0.50 %
Silicon, Si 62 %
62 %
Electrical Properties Metric English Comments
Volume Resistivity 1.4 ohm-cm
1.4 ohm-cm
Descriptive Properties Value Comments
C/Si Atomic Ratio 1.39
Filaments per tow 500