Material Notes:
Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Water Absorption 0.00 %
0.00 %
Loss On Ignition 0.50 %
0.50 %
Filament Diameter 14 - 26 µm
14 - 26 µm
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4500 MPa

@Temperature 23.0 °C
653000 psi

@Temperature 73.4 °F
Elongation at Break 5.5 %
5.5 %
Modulus of Elasticity 86.0 GPa
12500 ksi
Poissons Ratio 0.22
0.22
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 825 °C
1520 °F
Maximum Service Temperature, Inert 825 °C
1520 °F
Optical Properties Metric English Comments
Refractive Index 1.525
1.525