Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 3.90 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 3.90 - 4.10 g/cc
3.90 - 4.10 g/cc
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria..
Specific Gravity 3.90 g/cc
3.90 g/cc
Mixed; TM R050-16
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Specific Gravity 3.90 - 3.98 g/cc
3.90 - 3.98 g/cc
ASTM D792
Isoflon PTFE + 60% Bronze Polytetrafluoroethylene with 60% Bronze
Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for ..
Specific Gravity 3.90 g/cc
3.90 g/cc
ASTM D792
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers
Specific Gravity 3.90 g/cc
3.90 g/cc
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina
Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20.
Specific Gravity 3.90 g/cc
3.90 g/cc
Mixed; TM R050-16
Resinlab® SEC1222 Silver Filled Epoxy Adhesive
Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit..
Specific Gravity 3.90 g/cc
3.90 g/cc
Mixed; TM R050-16
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..
Copyright © lookpolymers.com All Rights Reserved