Material Notes:
Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, friable to tough, and contains no free chemicals. All oxides and dioxides are combined chemically as follows: Fe2O3Al2(SiO4)3. The iron and aluminum are partially replaceable by calcium, magnesium and manganese. There are three types- aluminum garnet, iron garnet & chromium garnet.Uses: Abrasive applications, water jet cutting, water filtration, tumbling media, non-skid surfaces, and semi-precious stone.Forms Available: Sintered pieces, targets, granules and various powder sizingsInformation provided by Reade Advanced Materials.
Physical Properties Metric English Comments
Specific Gravity 3.90 - 4.10 g/cc
3.90 - 4.10 g/cc
Bulk Density 2.40 g/cc
0.0867 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0 - 9.0
8.0 - 9.0
20°C
Thermal Properties Metric English Comments
Melting Point 1250 - 1315 °C
2280 - 2399 °F
Optical Properties Metric English Comments
Refractive Index 1.74 - 1.89
1.74 - 1.89
Descriptive Properties Value Comments
Color red to pink
Crystal Structure cubic