Polymer Property : Specific Gravity = 3.60 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 3.60 - 3.80 g/cc
3.60 - 3.80 g/cc
ASTM D792
P & P Technology EC-H Silver Copper Loaded Fluorosilicone
P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc..
Specific Gravity 3.60 - 4.40 g/cc
3.60 - 4.40 g/cc
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Specific Gravity 3.60 g/cc
3.60 g/cc
Parker Chomerics CHO-BOND® 1121 General Purpose Adhesive-Sealant Silver Silicone
Description: Xylene-free version of CHO-BOND 1038; rec. bond line thickness: > 0.18 mm; primer promotes adhesion CHO-BOND® 1121 is an electrically conductive, one-component silicone adhesive-sealan..
Specific Gravity 3.60 g/cc
3.60 g/cc
ASTM D792
Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Specific Gravity 3.60 g/cc
3.60 g/cc
Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System
Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interco..
Specific Gravity 3.60 g/cc
3.60 g/cc
Mixed
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy
TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc.
Specific Gravity 3.60 g/cc
3.60 g/cc
Atom Adhesives AA-DUCT 904 Epoxy Adhesive
AA-DUCT 904 is a single component, heat curing, conductive epoxy that was designed for ease in handling. This high performance conductive epoxy cures quickly at elevated temperatures making it ideal..