Material Notes:
TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 3.60 g/cc
3.60 g/cc
Mixed
Viscosity 62000 cP
62000 cP
Mixed (cp #52, 5 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
7 hrs ± 30 min @ 95°C
Adhesive Bond Strength 15.01 MPa
2177 psi
Lap shear, alum to alum, 1 hr @ 150°C
Thermal Properties Metric English Comments
CTE, linear 44.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
24.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
Below Tg
140 µm/m-°C

@Temperature 110 - 150 °C
77.8 µin/in-°F

@Temperature 230 - 302 °F
Above Tg
Glass Transition Temp, Tg 90.0 °C
194 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
60.0 min

@Temperature 125 °C
1.00 hour

@Temperature 257 °F
Shelf Life 6.00 Month
6.00 Month
At 5°C
12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Color Silver
Working Life, months 3