Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.22 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.22 g/cc
2.22 g/cc
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D792
Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 513 Perfluoroelastomer
Chemraz® 513 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contamination is required. This material offers excellen..
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 517 Perfluoroelastomer
Greene Tweed’s Chemraz® 517, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 517 has a Shore A..
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 537 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D297
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer
Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance an..
Specific Gravity 2.22 - 2.26 g/cc
2.22 - 2.26 g/cc
ASTM D792
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1)
Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityInformation provided by Isoflon.
Specific Gravity 2.22 g/cc

@Temperature 25.0 °C
2.22 g/cc

@Temperature 77.0 °F
Dow Corning SE 9184 WHITE RTV
One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning
Specific Gravity 2.22 g/cc
2.22 g/cc
Asahi Glass Fluon® CD1 PTFE Coagulated Dispersion Powder
Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc.
Specific Gravity 2.22 g/cc
2.22 g/cc
Asahi Glass Fluon® PA1020Z 20% Glass Fiber, PTFE Filled Compound
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D4745
3M Dyneon™ CC103 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D4745
3M Dyneon™ CC605 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 25% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company
Copyright © lookpolymers.com All Rights Reserved