Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance and lwo extractables similar to PTFE. Providing the lowest temperature sealing properties of any perfluoroelastomer on the market (-22°F, -30°C), Chemraz SD517 is an ideal seal component for sub-ambient mechanical seal applications and is the preferred alternative to encapsulated O-rings. With its white color, Chemraz SD517 meets the needs of applications requiring non-black elastomers.Chemraz SD517’s many features make it well suited for critical applications and difficult seal replacement locations where maximizing MTBR (mean time between replacement) is paramount.Chemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes.This product is FDA and USP Class VI compliant making it an ideal product for electrometric applications requiring regulatory compliance.Applications:Mechanical sealsValvesPumpsMixersFermentersBiomedical equipmentCouplingsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.22 g/cc
2.22 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D1414
Tensile Strength, Yield 3.72 MPa
540 psi
@50% Elongation; ASTM D1414
7.24 MPa
1050 psi
@100% Elongation; ASTM D1414
Compression Set 25 %
25 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color White