Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.22 g/cc | 2.22 g/cc | |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D792 |
Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 513 Perfluoroelastomer Chemraz® 513 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contamination is required. This material offers excellen.. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 517 Perfluoroelastomer Greene Tweed’s Chemraz® 517, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 517 has a Shore A.. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 537 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance an.. |
|||
Specific Gravity | 2.22 - 2.26 g/cc | 2.22 - 2.26 g/cc | ASTM D792 |
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1) Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityInformation provided by Isoflon. |
|||
Specific Gravity | 2.22 g/cc @Temperature 25.0 °C |
2.22 g/cc @Temperature 77.0 °F |
|
Dow Corning SE 9184 WHITE RTV One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | |
Asahi Glass Fluon® CD1 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | |
Asahi Glass Fluon® PA1020Z 20% Glass Fiber, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D4745 |
3M Dyneon™ CC103 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 15% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Specific Gravity | 2.22 g/cc | 2.22 g/cc | ASTM D4745 |
3M Dyneon™ CC605 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 25% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |