Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | >= 2.00 g/cc | >= 2.00 g/cc | |
Parker Chomerics CHO-BOND 1067, Part B Conductive Powder Information provided by Chomerics |
|||
Specific Gravity | >= 2.00 g/cc | >= 2.00 g/cc | |
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Bio.. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D4894 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D-792 |
Glastic GLASTHERM HT250 Insulation Sheet Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbesto.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump effi.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
Spartech Sound X Noise Abatement Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 190nl-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 205-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 251-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Silberline Aquavet® 651-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
Ecomass® 1080BI64 Filled Polyamide Nontoxic alternative compound for weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Po.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | ASTM D792 |
3M Dyneon™ THV 500GZ Fluorothermoplastic Granules THV 500G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature proce.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
3M Dyneon™ TFE 90Z Peroxide Cure Perfluoroelastomer 3M™ Dyneon™ Peroxide Cure Perfluoroelastomer PFE 90Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It is classif.. |
|||
Specific Gravity | >= 2.00 g/cc | >= 2.00 g/cc | |
Parker Chomerics CHO-BOND 1053, Part A Conductive Powder Information provided by Chomerics |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | Part A; TM R050-16 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |