Polymer Property : Specific Gravity = 2.12 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.05 - 2.12 g/cc
2.05 - 2.12 g/cc
ASTM D792
Isoflon PTFE + 25% Carbon Polytetrafluoroethylene with 25% Carbon
Properties:Improved compression and wear resistanceGood thermal conductivityLow permeabilityImproved coefficient of thermal expansion when combined with ceramicApplications: Seals recommended for h..
Specific Gravity 2.11 - 2.12 g/cc
2.11 - 2.12 g/cc
ASTM D792
Adamas Adalon® 413 PTFE, 20% PPS
Information provided by Adamas, HPM
Specific Gravity 2.10 - 2.12 g/cc
2.10 - 2.12 g/cc
ASTM D792
Asahi Glass Fluon® P-63P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.10 - 2.12 g/cc
2.10 - 2.12 g/cc
ASTM D792
Asahi Glass Fluon® P-810UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Specific Gravity 2.09 - 2.12 g/cc
2.09 - 2.12 g/cc
ASTM D792
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled
Information provided by Adamas, HPM