Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.09 g/cc | 2.09 g/cc | ASTM D1505 |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Specific Gravity | 2.09 g/cc | 2.09 g/cc | ASTM D1505 |
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Specific Gravity | 2.09 g/cc | 2.09 g/cc | ASTM D1505 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Specific Gravity | 2.09 g/cc | 2.09 g/cc | ASTM D1505 |
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Specific Gravity | 2.09 g/cc | 2.09 g/cc | ASTM D1505 |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Specific Gravity | 2.09 - 2.15 g/cc | 2.09 - 2.15 g/cc | ASTM D 792 |
Karina 1100/1075 IE MBPP White Color Concentrate Filled white concentrate recommended for olefin applications. Recommended usage from 5%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 2.09 - 2.12 g/cc | 2.09 - 2.12 g/cc | ASTM D792 |
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled Information provided by Adamas, HPM |