Polymer Property : Specific Gravity = 2.05 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.05 g/cc
2.05 g/cc
ASTM D792
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Specific Gravity 2.05 g/cc
2.05 g/cc
ASTM D792
Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Specific Gravity 2.05 - 2.12 g/cc
2.05 - 2.12 g/cc
ASTM D792
Isoflon PTFE + 25% Carbon Polytetrafluoroethylene with 25% Carbon
Properties:Improved compression and wear resistanceGood thermal conductivityLow permeabilityImproved coefficient of thermal expansion when combined with ceramicApplications: Seals recommended for h..
Specific Gravity 2.05 g/cc
2.05 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 656 Perfluoroelastomer
Chemraz® 656 is a low durometer perfluoroelastomer primarily designed for Bonded Slit Valve gates and special engineered applications such as low sealing forces/tolerance stickups where softer ma..
Specific Gravity 2.05 g/cc
2.05 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT
LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity.