Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled  (disco

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne™ Corporation
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
24 Hr; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Ash 65 %
65 %
ASTM D2584
Mechanical Properties Metric English Comments
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 24.1 GPa
3500 ksi
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 22.8 GPa
3300 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D648
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 271 °C
520 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 299 - 332 °C
570 - 630 °F
Mold Temperature 121 - 149 °C
250 - 300 °F
Drying Temperature 121 °C
250 °F