Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluoropolymer but need excellent flexibility or excellent transparency. THVP 2030GZ is processed at low temperatures, but exhibits a slightly higher melt point and end-use temperature capability than THV 220.Features and Benefits: Most flexible grade of THV Bondable to itself and other substrants E-beam crosslinkable Low flammability Highest transparency of the THV grades Processing profile allows co-processing with other plastics, hydrocarbon elastomers and acrylicsInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D792
Bulk Density 0.950 g/cc
0.0343 lb/in³
ASTM D1895
Melt Index of Compound 25 g/10 min

@Load 5.00 kg,
Temperature 265 °C
25 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
ASTM D1708
Elongation at Break 535 %
535 %
ASTM D1708
Flexural Modulus 0.0320 GPa
4.64 ksi
two inch span; ASTM D790
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
ASTM D4591
Optical Properties Metric English Comments
Refractive Index 1.35
1.35
nD
Transmission, Visible 91 %

@Thickness 0.254 mm,
Wavelength 500 nm
91 %

@Thickness 0.0100 in,
Wavelength 500 nm
film
IR Transmittance 92 %

@Thickness 2.34 mm,
Wavelength 750 nm
92 %

@Thickness 0.0920 in,
Wavelength 750 nm
film
UV Transmittance 75 %

@Thickness 0.254 mm,
Wavelength 220 nm
75 %

@Thickness 0.0100 in,
Wavelength 220 nm
film
90 %

@Thickness 0.254 mm,
Wavelength 350 nm
90 %

@Thickness 0.0100 in,
Wavelength 350 nm
film
Descriptive Properties Value Comments
Form Pellets