Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer MRC Polymers
Trade Name MAXNITE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
Water Absorption 0.060 %
0.060 %
ASTM D 570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D 696
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D 785
Tensile Strength 117.2 MPa
17000 psi
ASTM D 638
Elongation at Break 3.0 %
3.0 %
ASTM D 638
Flexural Strength 182.8 MPa
26510 psi
ASTM D 790
Flexural Modulus 6.89 GPa
999 ksi
ASTM D 790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
430 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ASTM D 648