Axiall 4420 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 4420 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High speed TWP wire harness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 39 - 45
39 - 45
delayed; ASTM D-2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 300 %
300 %
ASTM D-638
100% Modulus 0.0148 GPa
2.15 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F