Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-10GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 0.25 %
0.25 %
24 hr. Immersion, -; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.79 GPa
550 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
205 °F
Annealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 221 - 238 °C
430 - 460 °F
Molding
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
2 hrs
Descriptive Properties Value Comments
Product Form Pellets
Copyright © lookpolymers.com All Rights Reserved