Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Asahi Glass Company
Trade Name Lumiflon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-302 has a UV absorber that makes it unique in the Lumiflon line. The LF-302 is used as a clear coat over plastic, metals, and paints.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.09 g/cc
1.05 - 1.09 g/cc
Viscosity Measure 239 - 418 cSt
239 - 418 cSt
Molecular Weight 20000 g/mol
20000 g/mol
Mechanical Properties Metric English Comments
Impact 40
40
cm, DuPont Impact (1kg x 1/2 in.)
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Optical Properties Metric English Comments
Gloss 81 %
81 %
Chemical Properties Metric English Comments
Acid Value 0.00
0.00
Descriptive Properties Value Comments
Appearance Transparent
Erichsen Test 0
N.V. wt % 50±1
OH Value mg KOH/g 52
Pencil Hardness 4H/F
Solvent Xylene
T-bend test (no cracking) 3T
Xylol Rubbing Test >200 times