Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.927 g/cc | 0.927 g/cc | |
Teknor Apex TruVis Esters™ DOA Di-Octyl Adipate |
|||
Specific Gravity | 0.927 g/cc | 0.927 g/cc | ASTM D792 |
Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Specific Gravity | 0.927 g/cc | 0.927 g/cc | ISO 1183 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |
|||
Specific Gravity | 0.927 g/cc | 0.927 g/cc | ISO 1183 |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Specific Gravity | 0.927 g/cc | 0.927 g/cc | ISO 1183 |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion .. |
|||
Specific Gravity | 0.927 g/cc | 0.927 g/cc | ASTM D792 |
Elastocon TPE Technologies Elastocon® OF75 Thermoplastic Elastomer Elastocon® OF75 is a natural thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a reduced coefficient of friction. Ela.. |