Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.927 g/cc
0.927 g/cc
Viscosity 2.3 cP

@Temperature 100 °C
2.3 cP

@Temperature 212 °F
8.2 cP

@Temperature 40.0 °C
8.2 cP

@Temperature 104 °F
Viscosity Measurement 88.0
88.0
Viscosity Index
Thermal Properties Metric English Comments
Pour Point -67.0 °C
-88.6 °F
Flash Point 195 °C
383 °F
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
mg KOH/g
Descriptive Properties Value Comments
Appearance Clear
Color 50
Pt/Co Scale
Ester Content (%), min 99
Moisture (ppm), max 500