Polymer Property : Specific Gravity = 0.875 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.875 g/cc
0.875 g/cc
ASTM D1505
LG Chemical LC565 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Specific Gravity 0.875 - 0.905 g/cc
0.875 - 0.905 g/cc
BAM 1014
Kraton® G2705 GU (SEBS) Compound
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct..
Specific Gravity 0.875 g/cc
0.875 g/cc
Indium Corp. Indalloy® 84004 Flux #4-0A Clear Liquid Flux
Indalloy Flux #4-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o..
Specific Gravity 0.875 g/cc
0.875 g/cc
15.6°C; ASTM D1298
ExxonMobil Teresstic 46
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Specific Gravity 0.875 g/cc
0.875 g/cc
ConocoPhillips Syncon® 220 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Specific Gravity 0.875 g/cc

@Temperature 25.0 °C
0.875 g/cc

@Temperature 77.0 °F
Dow Corning Z-6341 SILANE
Dow Corning® Z-6341 Silane is high purity, undiluted N-octyltriethoxy-silane. When diluted with an appro-priate solvent, it can be used in the formulation of water repellent prod-ucts. Upon proper ..
Specific Gravity 0.875 g/cc
0.875 g/cc
ExxonMobil Mobil Vaprotec Light
Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light..
Specific Gravity 0.875 g/cc
0.875 g/cc
15.6°C; ASTM D1298
ExxonMobil Teresstic 46
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Specific Gravity 0.875 g/cc
0.875 g/cc
60°F
ConocoPhillips El Mar® Grade 15W-40 Mid Ash Supreme Oil
Description: Conoco El Mar® Mid Ash Supreme Oil is a premium-quality, mid ash gas engine oil recommended for naturally aspirated and moderately to highly turbocharged four-cycle gas engines, such a..
Specific Gravity 0.875 g/cc
0.875 g/cc
60°F
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40
Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi..
Specific Gravity 0.875 g/cc
0.875 g/cc
ExxonMobil Mobil Vaprotec Light
Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light..