Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.875 - 0.905 g/cc | 0.875 - 0.905 g/cc | BAM 1014 |
Kraton® G2705 GU (SEBS) Compound Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct.. |